M. Abdollahy; S. M. J. Koleini; A. Ghaffari
Abstract
Cyanidation process is one of the most important and widespread hydrometallurgical technologies used in the extraction of gold and silver from ores and concentrates. Some of the most effective parameters on cyanide leaching are sodium cyanide concentration, dissolved oxygen, solid percent, pH, particle ...
Read More
Cyanidation process is one of the most important and widespread hydrometallurgical technologies used in the extraction of gold and silver from ores and concentrates. Some of the most effective parameters on cyanide leaching are sodium cyanide concentration, dissolved oxygen, solid percent, pH, particle size, retention time and agitation speed. In this article the effect of these parameters on the recovery of gold, silver and mercury from Pouya Zarkan Aghdareh ore has been studied to determine the optimum conditions using Taguchi exprimental design method. The experiments at the screening step based on L16 orthogonal array indicated that the effective parameters on gold, silver and mercury recovery such as sodium cyanide, pH, solid percent in pulp, d80 and retention time were obtained equal to 900 g/t ore, 10, 42%, 53 μm and 30 h, respectively. The experiments at the optimization step based on L18 orthogonal array indicated that d80 on gold recovery and retention time on silver and mercury recovery were the most effective parameters. Finally the optimum conditions for gold, silver and mercury recovery were obtained for parameters such as sodium cyanide, pH, solid percent in pulp, d80 and retention time equal to 1000 g/t ore, 10.3, 46%, 37 μm and 40 h, respectively. At this conditions gold, silver and mercury recovery were equal to 91.42±1.02, 54.31±1.24 and 19.50±0.66 percent, respectively.
M. Abdollahy; A. Raissi; H. Naderi
Abstract
An investigation on beneficiation of Lakhshak antimony ore was carried out using flotation methods. The grade of antimony in representative sample was 17.23%. The most important minerals were stibnite, quartz and pyrite and the degree of liberation of stibnite was found to be 700 micrometer. The raw ...
Read More
An investigation on beneficiation of Lakhshak antimony ore was carried out using flotation methods. The grade of antimony in representative sample was 17.23%. The most important minerals were stibnite, quartz and pyrite and the degree of liberation of stibnite was found to be 700 micrometer. The raw material was divided into three size fractions and beneficiation of fine size fraction (-210+38 m) was floated. The grade of mentioned fraction was 20.50 %. Taguchi method was used in flotation tests and optimum conditions were determined as follows: CuSO4 (1700g/t) as an activator, potassium etyle xanthate (900 g/t) as a collector, MIBC as a frother, pulp density 22% and grain size -150+38 m. All the experiments were carried out at pH = 6.8. As a result the grade and recovery of antimony was obtained 38% (Sb) and 91% respectively.